Research Article - (2015) Volume 5, Issue 3

Capacity Fade Study of LiCo0.4Al0.1Mn1.5O4 Cathode Material for Li-Ion Batteries Cycled at Low Discharge Rates

Nayaka GP1, Pai KV1*, Manjanna J2*, Anjaneya KC2, Periasamy P3 and Tripathi VS4
1Department of Industrial Chemistry, Kuvempu University, Shankaraghatta, 577 451, India, E-mail: gp.nayaka@ncl.res.in
2Department of Chemistry, Rani Channamma University, Belagavi, 591 156, India, E-mail: gp.nayaka@ncl.res.in
3Central Electrochemical Research Institute, Karaikudi 630 006, India, E-mail: gp.nayaka@ncl.res.in
4Chemistry Group, Bhabha Atomic Research Centre, Mumbai 400 085, India, E-mail: gp.nayaka@ncl.res.in
*Corresponding Author(s):